Conditions: temp:0.00; pressure:0.00; stir:; See reaction.notes.procedure_details.
Procedure: 400 g montanic acid (Hoechst-Wachs S), 97 g glycerol (5% excess) and 0.5 g tin powder were reacted as in Example 1. A yellow, brown-tinged hard wax having a dropping point of 84.2° C. was obtained. a dropping point of 84.2° C. was obtained
Source ID: ord-944a178a9d084de2b20ed9e67ddd4aba